1. Cov txheej txheem Casting thiab Metallurgical
Advanced casting manufacturing technologies thiab ua cov cuab yeej-xws li tswj solidification, nplua-grain ua, laser sib sau / kho, thiab hnav-resistant casting hom kev kawm-yog tsis tu ncua raug tsim thiab refined. Kev txhim kho rau cov thev naus laus zis uas twb muaj lawm txhim kho qhov zoo sib xws thiab kev ntseeg siab ntawm ntau yam superalloy casting khoom.
Superalloys uas muaj me me rau tsis muaj txhuas lossis titanium feem ntau yog melted siv hluav taws xob arc rauv los yog tsis-vacuum induction furnaces. Rau superalloys nrog siab aluminium thiab titanium cov ntsiab lus, melting nyob rau hauv lub atmospheric ib puag ncig ua rau nws nyuaj rau tswj lub caij poob thiab ua rau kom muaj roj ntau ntxiv thiab inclusion kab mob; Yog li ntawd, lub tshuab nqus tsev melting yog yuav tsum tau. Txhawm rau txo cov ntsiab lus suav nrog thiab txhim kho kev faib khoom thiab kev sib koom ua ke ntawm ingot crystallization qauv, cov txheej txheem duplex sib txuas ua ke thawj melting thiab theem nrab remelting yuav raug ua hauj lwm. Cov txheej txheem melting tseem ceeb muaj xws li hluav taws xob arc rauv, lub tshuab nqus tsev induction, thiab lub tshuab nqus tsev induction cua sov; Lwm txoj hauv kev remelting muaj xws li lub tshuab nqus tsev siv hluav taws xob hluav taws xob thiab cov hluav taws xob hluav taws xob remelting furnaces.
Ingots ntawm kev daws teeb meem muaj zog alloys thiab alloys uas tsis tshua muaj txhuas thiab titanium cov ntsiab lus (tag nrho Al + Ti < ~ 4.5%) tuaj yeem tawg ntawm forging. Alloys nrog siab aluminium thiab titanium cov ntsiab lus feem ntau xav tau extrusion lossis dov rau thawj zaug tawg, ua raws li kub dov rau hauv cov khoom tiav; qee cov khoom tau dhau los ua qhov txias txias los yog kos duab txias. Loj-inch alloy ingots los yog pancake-puab forgings yuav tsum tau ua nrog hydraulic presses los yog high-speed forging hydraulic presses.
2. Crystallization Metallurgical txheej txheem
Txhawm rau txo lossis tshem tawm cov ciam teb ntawm cov qoob loo perpendicular rau qhov kev ntxhov siab axis-zoo li txo qis lossis tshem tawm cov txheej txheem porosity-directional solidification txheej txheem tau tsim nyob rau xyoo tas los no. Cov txheej txheem no yuav ua rau cov nplej loj hlob raws ib qho kev coj ua crystallographic thaum lub sij hawm solidification, uas ua rau cov kab sib npaug ntawm cov nplej tsis pub hla hla ciam teb. Lub hauv paus yuav tsum tau ua kom tiav cov kev taw qhia solidification yog tsim thiab tswj kom txaus siab axial kub gradient thiab zoo axial kub dissipation ntawm cov kua thiab solidus kub. Tsis tas li ntawd, txhawm rau tshem tawm cov ciam teb tag nrho, kev tshawb fawb rau hauv cov txheej txheem tsim khoom rau ib leeg-crystal blades kuj tseem tsim nyog . 3. Cov txheej txheem hmoov hlau
Cov txheej txheem hmoov metallurgy feem ntau yog siv los tsim cov nag lossis daus-muaj zog thiab oxide-dispersion-strengthened superalloys. Cov txheej txheem no imparts plasticity-los yog superplasticity-rau cam khwb cia superalloys uas tsis yog-deformable.
4. Txhim kho cov txheej txheem
(1) Solid-Solution Strengthening
Lub matrix muaj zog los ntawm kev ntxiv cov ntsiab lus nrog atomic qhov sib txawv ntawm cov hlau matrix (xws li chromium, tungsten, molybdenum) kom induce lattice distortion; los ntawm kev ntxiv cov ntsiab lus uas txo cov stacking-fault zog ntawm alloy matrix (xws li, cobalt); thiab los ntawm kev ntxiv cov ntsiab lus uas retard diffusion tus nqi ntawm matrix ntsiab (xws li, tungsten, molybdenum).
(2) Ua kom muaj zog los nag
Lub alloy yog ntxiv dag zog los ntawm kev laus kev kho mob, uas ua rau cov nag lossis daus ntawm ib theem thib ob (xws li ', ", los yog carbides) los ntawm supersaturated solid tov. Lub 'theem sib koom tib lub ntsej muag-centered cubic (FCC) qauv raws li lub matrix, muaj ib tug zoo xws li lattice tas li, thiab yog coherent nrog cov siv lead ua lattice; consequently, nyob rau hauv lub uniformity ntawm lub teeb, consequently. impeding dislocation txav thiab muab qhov tseem ceeb ntxiv dag zog rau lub 'theem yog A3B-hom intermetallic compound, qhov twg A sawv cev rau npib tsib xee los yog cobalt, B sawv cev rau txhuas, titanium, niobium, tantalum, vanadium, los yog tungsten, thiab chromium, molybdenum, los yog hlau muaj peev xwm nyob rau hauv lub A yog nickel 3 qhov chaw. Ti).
Lub zog ntawm cov nyhuv ntawm 'theem tuaj yeem txhim kho los ntawm cov hauv qab no txhais tau tias:
① nce qhov ntim feem ntawm 'theem;
② Kho cov lattice mismatch ntawm 'theem thiab matrix kom ua tiav kev txhawb nqa los ntawm kev sib koom ua ke;
③ Ntxiv cov ntsiab lus xws li niobium thiab tantalum los ua kom muaj zog tiv thaiv theem ciam teb (APB) lub zog ntawm 'theem, yog li txhim kho nws qhov tsis kam mus rau dislocation shearing;
④ Ntxiv cov ntsiab lus xws li cobalt, tungsten, thiab molybdenum los ua kom lub zog ntawm lub cev ntawm 'theem. Lub "theem muaj lub cev-centered tetragonal (BCT) qauv) nrog cov muaj pes tsawg leeg Ni3Nb. Vim yog qhov tseem ceeb lattice mismatch ntawm lub "theem thiab lub matrix, ntau coherency strain induced, imparting siab yield zog rau lub alloy; Txawm li cas los xij, qhov kev ua kom muaj zog txo qis qis heev ntawm qhov kub siab tshaj 700 degree. Cobalt-based superalloys feem ntau tsis muaj cov theem tab sis yog hloov los ntawm carbides.